Polymer Property : Electrical Resistivity = 0.0000900 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 200 °C
0.0000900 ohm-cm

@Temperature 392 °F
Outokumpu 2205 Duplex Stainless Steel
Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t..
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 200 °C
0.0000900 ohm-cm

@Temperature 392 °F
Outokumpu SAF 2304® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 200 °C
0.0000900 ohm-cm

@Temperature 392 °F
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 20.0 °C
0.0000900 ohm-cm

@Temperature 68.0 °F
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi..
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 20.0 °C
0.0000900 ohm-cm

@Temperature 68.0 °F
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel
Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r..
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 20.0 °C
0.0000900 ohm-cm

@Temperature 68.0 °F
Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel
CLI SIRIUS S15 grade is a fully austenitic stainless steel containing 21 Cr, 1.7 Si, 0.17 N and Rare Earth elements (Cerium, Lanthanum,...etc) which make the alloy particularly well designed for hig..
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 20.0 °C
0.0000900 ohm-cm

@Temperature 68.0 °F
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42
Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0...
Electrical Resistivity 0.0000900 ohm-cm
0.0000900 ohm-cm
Goodfellow Nickel 78/Boron 14/Silicon 8 Alloy
Information provided by Goodfellow.
Electrical Resistivity 0.0000900 ohm-cm

@Temperature 200 °C
0.0000900 ohm-cm

@Temperature 392 °F
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..