Thermal Properties Metric English Comments
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
c direction
MarkeTech Rutile (TiO2) Fiber Optic Crystal
More chemically and physically resistant than Yttrium Vanadate. Large birefringence. Used for fiber optic beam displacers and optical isolators. Grown by Vernull method. Transmission range 500 to..
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel SIRIUS 800 H+ Heat Resistant Alloy
Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t..
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42
Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0...
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43
Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
Momentive Performance Materials Niobium Carbide (NbC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel SIRIUS 800 Heat Resistant Alloy
Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t..
Thermal Conductivity 13.0 W/m-K

@Temperature 100 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle..
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 - 100 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
CeramTec Ziralit Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec's Zirconia Toughened Alumina (Ziralit) provides excellent strength, excellent temperature performance, and superior toughness. It has enhanced performance for high quantity volume productio..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek Alumina-Zirconia Composite, AZ-25
Information provided by CoorsTek.
Thermal Conductivity 13.0 - 14.6 W/m-K
90.2 - 101 BTU-in/hr-ft²-°F
as built, XY direction
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing
EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to ..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy
Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at..
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy
Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at..
Thermal Conductivity 13.0 W/m-K

@Temperature 20.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel SIRIUS 800 H Heat Resistant Alloy
Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe..
Thermal Conductivity 13.0 W/m-K

@Temperature 85.0 °C
90.2 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 39 Bismuth Solder Alloy
Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C)
High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir..