Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name CLC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized corrosion. The grade is stabilized by the addition of Titanium that avoids intergranular corrosion and ensures good mechanical properties at room and elevated temperature. Alloy CLC 17-12-2Ti is an austenitic microstructure grade, free of deleterious carbide precipitations but containing CNTi precipitations on grain boundaries. The grain is regularly fine and contains some residual ferrite (approx 4%) after solution annealing (1050-1150°C – 1922-2102°F) and water quenching. The CLC 17-12-2Ti steel resists much better to wet atmosphere or solution containing chloride or fluoride addition. The steel is not seawater resistant. The alloy may be used in diluted chloridric or sulphuric acids at low temperature (= 330°C - 626°F) as well as in sour organic solutions. The grade is also well known for its high ductility, particularly when considering cold forming.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 560 MPa
81200 psi
Typical
520 - 670 MPa
75400 - 97200 psi
Minimum Guaranteed
Tensile Strength, Yield >= 220 MPa

@Strain 0.200 %
>= 31900 psi

@Strain 0.200 %
>= 260 MPa

@Strain 1.00 %
>= 37700 psi

@Strain 1.00 %
270 MPa

@Strain 0.200 %
39200 psi

@Strain 0.200 %
Typical
310 MPa

@Strain 1.00 %
45000 psi

@Strain 1.00 %
Typical
Elongation at Break 40 - 60 %
40 - 60 %
Creep Strength 250 MPa

@Temperature 600 °C,
Time 3.60e+6 sec
36300 psi

@Temperature 1110 °F,
Time 1000 hour
Modulus of Elasticity 200 GPa

@Temperature 20.0 - 100 °C
29000 ksi

@Temperature 68.0 - 212 °F
Poissons Ratio 0.299
0.299
Calculated
Shear Modulus 77.0 GPa

@Temperature 20.0 - 100 °C
11200 ksi

@Temperature 68.0 - 212 °F
Charpy Impact >= 125 J
>= 92.2 ft-lb
225 J
166 ft-lb
Typical
>= 100 J

@Temperature -196 °C
>= 73.8 ft-lb

@Temperature -321 °F
188 J

@Temperature -196 °C
139 ft-lb

@Temperature -321 °F
Typical
Thermal Properties Metric English Comments
CTE, linear 16.5 µm/m-°C

@Temperature 20.0 - 100 °C
9.17 µin/in-°F

@Temperature 68.0 - 212 °F
17.5 µm/m-°C

@Temperature 20.0 - 200 °C
9.72 µin/in-°F

@Temperature 68.0 - 392 °F
18.0 µm/m-°C

@Temperature 20.0 - 300 °C
10.0 µin/in-°F

@Temperature 68.0 - 572 °F
19.0 µm/m-°C

@Temperature 20.0 - 500 °C
10.6 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.500 J/g-°C

@Temperature 20.0 - 100 °C
0.120 BTU/lb-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 15.0 W/m-K

@Temperature 20.0 - 100 °C
104 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Component Elements Properties Metric English Comments
Carbon, C 0.050 %
0.050 %
Chromium, Cr 17 %
17 %
Iron, Fe 71.25 - 71.7 %
71.25 - 71.7 %
As remainder
Molybdenum, Mo 2.1 %
2.1 %
Nickel, Ni 11 %
11 %
Titanium, Ti 0.25 - 0.70 %
0.25 - 0.70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000750 ohm-cm

@Temperature 20.0 - 100 °C
0.0000750 ohm-cm

@Temperature 68.0 - 212 °F