Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
Outokumpu 4303 Cr-Ni Austenitic Stainless Steel Good corrosion resistance with excellent drawing properties.Applications: Suitable for cold formed components where good workability is required. Fasteners, studs.Available in hot rolled plate (Qua.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
MarkeTech MC-LD and MC-MD Ultra High Temperature Machinable Ceramics For very high temperatures or where thermal conductivity or thermal shock is important, these machinable alkaline/alkaline earth zirconium phosphate ceramics (NaZr2P3O12 or BaZr4P6O24) are recommend.. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 20.0 °C |
0.120 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL.. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 20.0 °C |
0.120 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b.. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 20.0 °C |
0.120 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
Special Metals NILO® 365 Controlled-Expansion Alloy For the manufacture of tooling for composites, the NILO® nickel-iron alloys offer a unique combination of matched thermal expansion to avoid warping during the curing cycle, along with strength, .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 201 Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 304 Austenitic Stainless steel AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. .. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 35% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 52% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum AL 20™ Plate Specialty Steel The N08020 alloy has been available for many years and has found applications in many environments, such as in chlorides and in sulfuric and sulfurous acids.Although AL 20 alloy was developed for im.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 0% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 316 Austenitic Stainless steel AK Steel 316 contains molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated tempe.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum AL 800H™ Nickel-Base Alloy, UNS N08810 AL 800H alloy is nickel-iron-chromium alloys designed to resist oxidation and carburization at elevated temperatures. The nickel content makes the alloy highly resistant both to chloride stress-cor.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 50% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 0% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 20% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 40% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Type 348 (UNS S34800) AL 348 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Type 347 (UNS S34700) AL 347 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°.. |