Polymer Property : Tensile Strength, Ultimate = 670 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 520 - 670 MPa
75400 - 97200 psi
Minimum Guaranteed
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel
Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform ..
Tensile Strength, Ultimate 520 - 670 MPa
75400 - 97200 psi
Minimum Guaranteed
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel
CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co..
Tensile Strength, Ultimate 520 - 670 MPa
75400 - 97200 psi
SSAB Tunnplat Domex® 460MC HSLA Steel
HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum ..
Tensile Strength, Ultimate 580 - 670 MPa
84100 - 97200 psi
ArcelorMittal Dual Phase 600 Very high strength steel, Hot Rolled Steel
Available in the following: HCT580X (uncoated)Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martens..
Tensile Strength, Ultimate 570 - 670 MPa
82700 - 97200 psi
ArcelorMittal HSLA 500 High strength low alloy steel for cold forming, Hot Rolled
Available in the following: S500MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w..
Tensile Strength, Ultimate 590 - 670 MPa
85600 - 97200 psi
ArcelorMittal FB 590 Hot rolled ferrite-bainite steel
Available in the following: uncoated (HDT590F)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: ..
Tensile Strength, Ultimate 590 - 670 MPa
85600 - 97200 psi
ArcelorMittal FB 590 HHE Hot rolled ferrite-bainite steel
Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: FB 450, 540, 560 and 590. This family of steel..