Mechanical Properties Metric English Comments
Charpy Impact 188 J

@Temperature -196 °C
139 ft-lb

@Temperature -321 °F
Typical
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel
CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co..