Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 125 J @Temperature -269 °C |
92.2 ft-lb @Temperature -452 °F |
Typical |
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
Charpy Impact | >= 125 J | >= 92.2 ft-lb | |
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co.. |
|||
Charpy Impact | >= 125 J @Temperature -196 °C |
>= 92.2 ft-lb @Temperature -321 °F |
|
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Charpy Impact | >= 125 J @Temperature -196 °C |
>= 92.2 ft-lb @Temperature -321 °F |
|
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |
|||
Charpy Impact | 125 J | 92.2 ft-lb | Austenitizing Temperature- 955°C |
Crucible Steel S7 (AISI S7) Tool Steel Crucible S7 is a shock resisting tool steel with excellent toughness and high strength, along with low to medium wear resistance. It has been widely used for many years to make chisels and punches w.. |
|||
Charpy Impact | 125 J | 92.2 ft-lb | Austenitizing Temperature- 955°C |
Crucible Steel S7 XL (Premium AISI S7) Tool Steel Crucible S7XL is a double refined, high purity grade of S7. The remelt operation produces a cleaner steel with a more uniform microstructure, offering the following advantages over conventional S7:B.. |
|||
Charpy Impact | >= 125 J @Temperature -196 °C |
>= 92.2 ft-lb @Temperature -321 °F |
|
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k.. |