Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Devcon
Trade Name Plastic Welder™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by ITW Devcon
Physical Properties Metric English Comments
Viscosity 56000 cP
56000 cP
Mixed Viscosity (Thixotropic gel)
Mechanical Properties Metric English Comments
Elongation at Break 5.0 - 15 %
5.0 - 15 %
Adhesive Bond Strength 20.7 MPa
3000 psi
lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002
Tensile Impact Strength 35.7 kJ/m²
17.0 ft-lb/in²
Peel Strength 2.63 - 3.51 kN/m
15.0 - 20.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
dry
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
dry
Processing Properties Metric English Comments
Cure Time 2.00 - 3.00 min
0.0333 - 0.0500 hour
Working time
8.00 - 10.0 min
0.133 - 0.167 hour
Fixture time
120 - 240 min
2.00 - 4.00 hour
Functional cure
Descriptive Properties Value Comments
Mix ratio (Resin:Hardener) 1:1
Users viewing this material also viewed the following: