Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 2.00 - 3.00 min | 0.0333 - 0.0500 hour | Aluminum, handling time |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | handling time |
Permabond TA436 Toughened Acrylic Adhesive PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength.. |
|||
Cure Time | 0.583 - 3.00 min | 0.00972 - 0.0500 hour | Average value: 1.63 min Grade Count:5 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Cure Time | 1.00 - 3.00 min @Temperature 204 - 260 °C |
0.0167 - 0.0500 hour @Temperature 399 - 500 °F |
|
Lord Adhesives Flocklok® 550P Flock Adhesive LORD Flocklok® 550P adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of uncured and semi-cured elastomers including EPDM, NR, CR and SBR. Flocked sub.. |
|||
Cure Time | 2.00 - 3.00 min | 0.0333 - 0.0500 hour | Working time |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White Information provided by ITW Devcon |
|||
Cure Time | 1.00 - 3.00 min @Temperature 140 - 160 °C |
0.0167 - 0.0500 hour @Temperature 284 - 320 °F |
|
Lucite International Colacryl ® TS1631 Acrylic Solution Resin Acrylic copolymer with reactive groupsA highly flexible resin with good handle. It exhibits good adhesion, resistance to ageing and light stability.Suggested Use: Coating and lamination of nylon and.. |
|||
Cure Time | 1.17 - 3.00 min | 0.0194 - 0.0500 hour | Gelation time |
Mitsui MILEXâ„¢ RN-2830MB Acrylic Rubber Modified Phenolic Resin The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad.. |
|||
Cure Time | 2.50 - 3.00 min @Temperature 150 °C |
0.0417 - 0.0500 hour @Temperature 302 °F |
|
Loctite® 3607 Pin Transfer Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te.. |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-30 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-31 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-32 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-33 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-34 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-35 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-36 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-37 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 1.00 - 3.00 min | 0.0167 - 0.0500 hour | Setting Time |
Chosun Refractories HSM-38 Heat-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 0.750 - 3.00 min | 0.0125 - 0.0500 hour | Time to Handling Strength |
3M Scotch-Weld™ ECI Gel General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |