Polymer Property : Tensile Impact Strength = 17.0 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 35.7 - 46.2 kJ/m²
17.0 - 22.0 ft-lb/in²
Average value: 41.3 kJ/m² Grade Count:9
Overview of materials for Methacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri..
Tensile Impact Strength 35.7 kJ/m²
17.0 ft-lb/in²
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Straw, Black
Information provided by ITW Devcon
Tensile Impact Strength 35.7 kJ/m²
17.0 ft-lb/in²
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White
Information provided by ITW Devcon