Multibase Multi-Flex® TPE A 6001 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 6001 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPE A 6001 is designed for gasket seals, rotational valves, and electrical applications as well as low friction applications. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min
1.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 sec; ASTM D-2240
Tensile Strength, Ultimate 13.8 MPa
2000 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
Flexural Modulus 0.0145 GPa
2.10 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 39.4 kN/m
225 pli
ASTM D624