Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Porene SP200 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer IRPC Polimaxx
Trade Name Porene
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF IRPC Polimaxx Porene SP200 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications:injection moldingHelmetsautomotiveelectroplatingpainting articles
Physical Properties Metric English Comments
Melt Flow 17 g/10 min
<br>@Load 10.0 kg,<br> Temperature 220 °C
17 g/10 min
<br>@Load 22.0 lb,<br> Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
109
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
ASTM D785
Tensile Strength, Ultimate 41.2 MPa
<br>@Temperature 23.0 °C
5970 psi
<br>@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 55.9 MPa
<br>@Temperature 23.0 °C
8110 psi
<br>@Temperature 73.4 °F
ASTM D790
Flexural Modulus 2.01 GPa
<br>@Temperature 23.0 °C
292 ksi
<br>@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 3.53 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
6.61 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
<br>@Thickness 6.35 mm
194 °F
<br>@Thickness 0.250 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
<br>@Thickness 6.35 mm
183 °F
<br>@Thickness 0.250 in
ASTM D648
Flammability, UL94 HB
<br>@Thickness 1.50 mm
HB
<br>@Thickness 0.0591 in
HB
<br>@Thickness 3.10 mm
HB
<br>@Thickness 0.122 in
Processing Properties Metric English Comments
Processing Temperature 190 - 240 °C
374 - 464 °F
Drying Temperature 80.0 - 90.0 °C
<br>@Time 7200 - 18000 sec
176 - 194 °F
<br>@Time 2.00 - 5.00 hour
Copyright © lookpolymers.com All Rights Reserved