Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 200 - 240 °C | 392 - 464 °F | Barrel Temperature |
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK40 is a high crystalline impact copolymer with high stiffness. This grade is especially developed for producing injection molded articles. The grade contains an antist.. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | Barrel Temperature |
SABIC PP 5703P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Processing Temperature | 230 - 240 °C | 446 - 464 °F | Extrusion cylinder temperature, C3 |
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Processing Temperature | 190 - 240 °C | 374 - 464 °F | |
IRPC Polimaxx Polene 2100N Polypropylene Block Copolymer CHARACTERISTICS: MEDIUM FLOW, HIGH STIFFNESSAPPLICATIONS: INJECTION MOLDING FOR HOUSEWARES, ELECTRICAL PARTS, AUTOPARTS |
|||
Processing Temperature | 190 - 240 °C | 374 - 464 °F | |
IRPC Polimaxx Polene 2340TC Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT FLOWABILITY, HIGH STIFFNESS, MEDIUM IMPACT, HEAT STABILITYAPPLICATIONS: INJECTION MOLDING FOR THIN WALL CONTAINERS : DRINKING CUPS, NOODLE CUPS |
|||
Processing Temperature | 190 - 240 °C | 374 - 464 °F | |
IRPC Polimaxx Polene 2500PC Polypropylene Block Copolymer CHARACTERISTICS: MEDIUM FLOW, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, AUTOPARTS, ICE CREAM CUPS, CONTAINERS |
|||
Processing Temperature | 190 - 240 °C | 374 - 464 °F | |
IRPC Polimaxx Porene GA300 Acrylonitrile Butadiene Styrene Applications: injection molding for electrical appliances, toys. |
|||
Processing Temperature | 230 - 240 °C | 446 - 464 °F | Extrusion cylinder temperature, C3 |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Processing Temperature | 160 - 240 °C | 320 - 464 °F | Bitumen modification |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | Metering Temperature, Extrusion |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 230 - 240 °C | 446 - 464 °F | C3 |
UBE 5033FDX27 Air Blown Nylon 6/66 Film Specialties: High slip typeMedium shrinkApplications: General purposeSuitable for Water cooling processProcessing: Sausage casings (Water)Big bag (Air blown)Information provided by UBE. |
|||
Processing Temperature | 160 - 240 °C | 320 - 464 °F | |
Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1200 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: flexible molding, handles, closures, household items, toys, variou.. |
|||
Processing Temperature | 190 - 240 °C | 374 - 464 °F | |
Cyclics CBT® 100 Thermoplastic Resin CBT® 100 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | |
Fainplast Compounds Ethylplus 600 Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid LDPEInformation provided by Fainplast Compounds.. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | |
Fainplast Compounds Ethylplus 619 LD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesBlack LDPE SheathingInformation provided by Fainplast.. |
|||
Processing Temperature | 200 - 240 °C | 392 - 464 °F | |
Eurotec® Tecolen® CP20 GB30 NL PPCP, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 210 - 240 °C | 410 - 464 °F | Extrusion Range |
Arkema Group Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7233 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | Injection molding |
BASF Elastoblend LP 9192 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | Injection molding |
BASF Elastollan S 70 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 60.0 - 240 °C | 140 - 464 °F | Injection |
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | Injection molding |
BASF Elastollan C 70 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | Injection molding |
BASF Elastollan S 74 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | Injection molding |
BASF Elastollan S 95 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | Injection molding |
BASF Elastollan S 60 AWH TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 180 - 240 °C | 356 - 464 °F | |
IRPC Polimaxx Porene KU900 Acrylonitrile Butadiene Styrene Applications:extrusion sheetrefrigerator door liners and inner box linerspicnic coolerssnow boatsluggage cases |