Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 41.2 MPa @Temperature 23.0 °C |
5970 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene GA400 Acrylonitrile Butadiene Styrene Applications:injection moldingelectrical applianceselectrical fansair conditionersfloppy disks |
|||
Tensile Strength, Ultimate | 41.2 MPa @Temperature 23.0 °C |
5970 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Porene SP200 Acrylonitrile Butadiene Styrene Applications:injection moldingHelmetsautomotiveelectroplatingpainting articles |
|||
Tensile Strength, Ultimate | 41.2 MPa | 5970 psi | ASTM D412 |
SK Chemicals SKYTHANE® 310 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 41.2 MPa | 5970 psi | ASTM D412 |
SK Chemicals SKYTHANE® 360D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 41.2 MPa | 5970 psi | ASTM D412 |
SK Chemicals SKYTHANE® S360D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 41.2 MPa | 5970 psi | ASTM D412 |
SK Chemicals SKYTHANE® UB310 Co-Extruding Adhesive Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Tensile Strength, Ultimate | 41.2 MPa | 5970 psi | ASTM D412 |
Lubrizol Estane® L194A Thermoplastic Polyurethane Type: Estane® L194A is a Shore 95A, polyester grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: AsiaInformation Provided by The Lubrizol Corporation |