Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.01 GPa | 292 ksi | ASTM D790 |
Hyosung Topilene J801R PP J801R Injection Special Purpose GradeApplications: Electric home applianceCharacteristics:High stiffnessLong-term heat resistanceInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 2.01 GPa @Thickness 3.20 mm |
292 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.01 GPa @Thickness 3.20 mm |
292 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI933 Co-Extrusion ASA Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | ASTM D790 |
Metton LMR M1539 Liquid Molding Resin Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can .. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | ASTM D790 |
Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene General Purpose ABS, SD 0150 grade, is a rigid thermoplastic with good processing characteristics. It is a high flow injection molding grade with considerable impact strength and medium heat deflec.. |
|||
Flexural Modulus | 2.01 GPa @Temperature 23.0 °C |
292 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene SP200 Acrylonitrile Butadiene Styrene Applications:injection moldingHelmetsautomotiveelectroplatingpainting articles |
|||
Flexural Modulus | 2.01 GPa @Temperature 23.0 °C |
292 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene SR101 Acrylonitrile Butadiene Styrene Applications:extrusion sheetrefrigerator door liners and inner box linerspicnic coolerssnow boatsluggage cases |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | ASTM D790 |
Metton LMR M2100VO Liquid Molding Resin Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can .. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-1010 PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-1010 PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-1030S PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HP-1000XA PC/ABS, Unreinforced PC/ABS material for automobile IP-coreInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | ASTM D790A |
Styron Magnumâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) High Impact, High Heat, Blow Molding ABSInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | ASTM D790 |
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-1030S PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | |
Zylog Hipolyene® 6251 Y M4 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | |
Zylog Hipolyene® 9221 XM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2mm/min; ASTM D790 |
Denka CL-430 Transparent Resin Polymer (MABS) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | 2mm/min; ASTM D790 |
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Modulus | 2.01 GPa @Thickness 6.40 mm |
292 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Flexural Modulus | 2.01 GPa @Thickness 6.40 mm |
292 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HI-34 ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Modulus | 2.01 GPa @Thickness 6.40 mm |
292 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Flexural Modulus | 2.01 GPa @Thickness 6.40 mm |
292 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HI-34 ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Modulus | 2.01 GPa @Temperature 23.0 °C |
292 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene KU900 Acrylonitrile Butadiene Styrene Applications:extrusion sheetrefrigerator door liners and inner box linerspicnic coolerssnow boatsluggage cases |
|||
Flexural Modulus | 2.01 GPa | 292 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinblend® A724 PC/PBT, High Impact Information from Shinkong Synthetic Fibers Corp. |