Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IPB Bicell® Cellular Polypropylene Sheet

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer IPB
Trade Name Bicell®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IPB Bicell® Cellular Polypropylene Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRecyclableFood approvedResistant to water and humidityGood resistance to grease, oils and most chemicalsSterilizableUses include packaging, including food, and displays.Property data reported here is based on PP raw material - not the formed sheet structure. Information provided by IPB Plastic Sheet Extrusion.
Physical Properties Metric English Comments
Density 0.907 g/cc
0.0328 lb/in³
ISO 1183
Water Absorption 0.02 %
0.02 %
ISO 62
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C
100 µin/in-°F
ASTM D696
Specific Heat Capacity 1.68 J/g-°C
0.402 BTU/lb-°F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
ISO 75
Vicat Softening Point 78.0 °C

@Load 5.10 kg
172 °F

@Load 11.2 lb
ISO 306
148 °C

@Load 1.02 kg
298 °F

@Load 2.25 lb
ISO 306
Electrical Properties Metric English Comments
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
Dielectric Constant 2.25

@Frequency 1.00e+6 Hz
2.25

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 70.0 kV/mm
1780 kV/in
ASTM D149
Dissipation Factor <= 0.000500

@Frequency 1.00e+6 Hz
<= 0.000500

@Frequency 1.00e+6 Hz
ASTM D150
Users viewing this material also viewed the following: