Polymer Property : Specific Heat Capacity = 0.402 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.68 J/g-°C
0.402 BTU/lb-°F
DSC
IPB Bicell® Cellular Polypropylene Sheet
Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe..
Specific Heat Capacity 1.68 J/g-°C
0.402 BTU/lb-°F
Dow Tyril® 125 SAN
Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov..