Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers MS 175 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CR750CL-02 Polypropylene, Random Copolymer, NX-8000 based COPYLENE™ CR750CL-02 is an easy molding, high melt flow random copolymer that has good see-through and contact clarity in injection molding applications and is formulated with advanced technology. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
Eastman Eastar DN102 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
SABIC PP 623B Polypropylene Random Co-polymer for Cast Film Product Description: PP 623B is a PP Random Copolymer grade specially designed for Cast PP (CPP) film extrusion. It contains slip agent and anti-block additives. PP 623B offers good heat weldabil.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting & Profile Extrusion ResinCharacteristics: High Stiffness, Good Impact Resistance, Very Low Odor & Taste Transfer, Designated for Uniloy Blowmol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | ASTM D 648 |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
LyondellBasell Petrothene® LM600500 High Density Polyethylene ApplicationsPETROTHENE LM 6005-00 resin is especially designed for water, milk, and juice bottles. It exhibits excellent rigidity and good processability.Regulatory StatusLM 6005-00 meets the requi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Flint Hills P9M6K-041A Specialty Impact Copolymer Polypropylene Features: Good clarity and impact resistance. Product does not contain animal derived components.Applications: Injection molding - durable goodsInformation provided by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Flint Hills P9R6K-054A Random Copolymer Polypropylene Features: Excellent clarity. High flow material. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement fo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
LG Chemical LUPOL HI5302A PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ISO 75 |
IPB Bicell® Cellular Polypropylene Sheet Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Lavergne VYSTYRENE PS 3904 High Impact Polystyrene Vystyrene PS 3904 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | ASTM D648 |
CPC - Vycom HITEC® HDPE High Density Polyethylene Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | ASTM D648 |
CPC - Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE) Grip-X is a UV stabilized high density polyethylene (HDPE) sheet formulated to meet demanding conditions of the marine industry. Grip-X is manufactured with a special surface treatment and stipulate.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Unannealed; ASTM Data |
Dow Prevail® 3150 ABS + Polyurethane PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | Unannealed; ASTM D648 |
Dow R7021-50RNA Polypropylene Random Copolymer Resin DOW™ R7021-50RNA Polypropylene Resin is a random copolymer designed for thin wall injection molding applications desiring high clarity.Main CharacteristicsGood impact propertiesExcellent opticsFast.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Unannealed; ISO 75-2/B |
Dow T702-12N Polypropylene Impact Copolymer Resin Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437C40L1 Calcium Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
BASF Novolen® 2500 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
BASF Polystyrol® 455 F WU Impact Grade Polystyrene (Europe) Very easy-flowing, impact-modified grade.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Cheng Yu Plastic IPS610BK Electric Conducting HIPS, Extrusion |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Extrusion Grade Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness for all extrusion applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.7 °C | 172 °F | Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Annealed; ISO 75-2A |
Total Lacqrene® 6631 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 - 98.0 °C | 172 - 208 °F | Average value: 87.8 °C Grade Count:12 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.8 °C | 172 °F | ASTM D 648 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |