Polymer Property : Vicat Softening Point = 298 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP CIP1001F Polypropylene
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP CQX8025 R2 Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP HBK15030 D Polypropylene, Multifiller High Gloss, Detergent Resistant
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T15040CR Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T16040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T4020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 5.001 kg
298 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANBLEND P AP2060 F30 PBT/ASA, Glass Fiber Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T10020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T16020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T3022D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T4030 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.02 kg
298 °F

@Load 2.25 lb
ISO 306
IPB Bicell® Cellular Polypropylene Sheet
Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe..
Vicat Softening Point 148 °C

@Load 1.02 kg
298 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope..
Vicat Softening Point 148 °C

@Load 1.02 kg
298 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope..
Vicat Softening Point 148 °C

@Load 1.02 kg
298 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope..
Vicat Softening Point 148 °C

@Load 0.999 kg
298 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND 4501 V0/D Flame Retardant PC - ABS
PC - ABS BlendFlame retardant class V0, PBDE and antimony free, with halogens, high impact resistance, very high thermal resistance, high gloss, good processabilityInformation provided by Cossa Poli..
Vicat Softening Point 148 °C

@Load 0.999 kg
298 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTACARB 1560 V0 Flame Retardant Polycarbonate
Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 148 °C

@Load 0.999 kg
298 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTACARB 1560 V0 HF Flame Retardant Polycarbonate
Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro..
Vicat Softening Point 148 °C

@Load 5.10 kg
298 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Makrolon® 2408 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Vicat Softening Point 148 °C

@Load 5.10 kg
298 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Makrolon® 2800 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Vicat Softening Point 148 °C

@Load 5.10 kg
298 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Vicat Softening Point 148 °C

@Load 5.10 kg
298 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Makrolon® 3258 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Wonderlite® PC-108U Polycarbonate - UV Stabilized
UV Stabilized
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Wonderlite® PC-122U Polycarbonate - UV Stabilized
UV Stabilized
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP HBK1501515 Polypropylene, Multifiller High Gloss
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T5038 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T5040DS Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant
Information provided by Polykemi AB
Vicat Softening Point 148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH T8020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB