Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
Plastcom SLOVAMID 6 GF 30 FRGG2 PA6, 30% glass fibre, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
Plastcom SLOVAMID 66 GF 25 FRG 5 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 66 GF 25 FRI 3 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 66 GF 35 FRI 3 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | STN EN 60243-2 |
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the .. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60243 |
Polimeri Europa Edistir N 1782 Polystyrene General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS f.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60243 |
Polimeri Europa Edistir N 1840 Polystyrene General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60243 |
Polimeri Europa Edistir N 2560 Polystyrene High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet
extrusion in ble.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
Polimeri Europa EDISTIR N1460 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,085-03 High molecular weight general purpose polystyrene with good mechanical strength. This grade is especially recomme.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
Polimeri Europa EDISTIR N1461 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-03 High molecular weight general purpose polystyrene with good mechanical strength. Well suitable for injection mold.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
Polimeri Europa EDISTIR N1671 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | Estimated from similar grades. ASTM D149 |
Solvay Specialty Polymers Algoflon® F 5 Polytetrafluoroethylene (PTFE) Algoflon® F 5 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for filled grades and in particular is recommended for compounds with glass fiber .. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | Estimated from similar grades. ASTM D149 |
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE) Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
Polyram PA500 Nylon 6.6, Flame Retardant Flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
Polyram PlusTek PA320G4 Nylon 6.6, 20% Glass Fiber, Flame Retardant 20% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
Polyram PlusTek PA324G6 Nylon 6.6, UL-94 V-0 30% Glass Fiber Self extinguishing (UL-94 V-0) 30% glass fiber reinforced polyamide 6.6 for component with high stiffness and dimensional stabilityInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149 |
Zeon Chemicals Zeonor® 750R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
Polyram PlusTek PB825G5 Nylon 6, 25% Glass Fiber 25% glass fiber reinforced, impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149, IEC 243 |
EPICHEM Epinyl PA 6 GF 30 ATP Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre, good toughness |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149, IEC 243 |
EPICHEM Epiryl PPO V0 Polyphenylene oxide Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | |
Covestro Bayblend® KU 1-1446 Polycarbonate/ABS Blend Good cold impact strength and fuel resistance.Applications: Automotive industry (interior and body parts).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated fr.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149, IEC 243 |
EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre filled |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® S 121 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® F6 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | IEC 60243 |
Polimeri Europa Edistir N 1910 Polystyrene Very easy flow general purpose polystyrene. Used for injection of thin-wall, multi-cavity, very fast-cycle mouldings and for sheet extrusion in glossy capping of HIPS and in blend with HIPS or clear.. |
|||
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | VDE 0303/4 |
Polyram PlusTek RA320G3 Nylon 6.6, 15% Glass Fiber, Flame Retardant 15% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |