Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.68 J/g-°C | 0.402 BTU/lb-°F | DSC |
IPB Bicell® Cellular Polypropylene Sheet Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe.. |
|||
Specific Heat Capacity | 1.68 J/g-°C | 0.402 BTU/lb-°F | |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |