Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ISO 75-1 |
Mytex Polymers 8224LW Polypropylene, Non-filled, Compounded Description: Mytex® 8224LW is a non-filled compounded polypropylene produced for automotive applications.Key Applications: Automotive exteriorInformation provided by Mytex Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers MS 175 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Method A; ASTM D648 |
Polymer Industries Densetec HMW Sheet Polymer Industries’ Densetec HMW is the extruded material needed when Densetec HDPE is not enough and Polyslick UHMW™ is not necessary. Densetec HMW has higher impact strength than HDPE and is mor.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
Eastman Eastar DN102 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ISO 75 |
Solvay Engineered Polymers SEQUEL® 2322 Engineered Polyolefin
(discontinued **) SEQUEL® 2322 engineered polyolefin is designed for mold-in-color automotive interior applications that require medium stiffness and good dimensional stability. This material exhibits excellent low.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
SABIC PP 623B Polypropylene Random Co-polymer for Cast Film Product Description: PP 623B is a PP Random Copolymer grade specially designed for Cast PP (CPP) film extrusion. It contains slip agent and anti-block additives. PP 623B offers good heat weldabil.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 6010 High Impact Polystyrene
(discontinued **) STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Chevron Phillips HiD® 9402 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting and Profile ResinCharacteristics: High Melt Strength - Larger Parts, Wide Range of Processing Conditions, High Stiffness and Impact Resistance,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting & Profile Extrusion ResinCharacteristics: High Stiffness, Good Impact Resistance, Very Low Odor & Taste Transfer, Designated for Uniloy Blowmol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
Reliance Industries Polypropylene - Talc filled Information provided by Reliance Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
LyondellBasell Petrothene® LM600500 High Density Polyethylene ApplicationsPETROTHENE LM 6005-00 resin is especially designed for water, milk, and juice bottles. It exhibits excellent rigidity and good processability.Regulatory StatusLM 6005-00 meets the requi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Flint Hills AP7810-HS Polypropylene Ultra High Impact Copolymer Features: Excellent stiffness and low temperature ductility.Applications: Injection Molding: Automotive interior energy management solutionsInformation Provided by Flint Hills Resources |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Flint Hills P9M6K-041A Specialty Impact Copolymer Polypropylene Features: Good clarity and impact resistance. Product does not contain animal derived components.Applications: Injection molding - durable goodsInformation provided by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Flint Hills P9R6K-054 Random Copolymer Polypropylene Excellent clarity. High flow material. Product does not contain any animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement for PET, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Flint Hills P9R6K-054A Random Copolymer Polypropylene Features: Excellent clarity. High flow material. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement fo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
LG Chemical LUPOL HI5302A PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ISO 75 |
IPB Bicell® Cellular Polypropylene Sheet Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
Lavergne VYSTYRENE PS 3904 High Impact Polystyrene Vystyrene PS 3904 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | unannealed; ASTM D648 |
Lendell Parapet GR-00100 PMMA, High Impact |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | ASTM D648 |
LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, medium high modulus, UV-stabilized, mineral-filled, blow molding and extrusion grade polypropylene copolymer, excellent impact and stiffness balance, good melt st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C @Thickness 3.20 mm |
172 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Unannealed; ASTM Data |
Dow Prevail® 3150 ABS + Polyurethane PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Unannealed; ISO 75-2/B |
Dow T702-12N Polypropylene Impact Copolymer Resin Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
BASF Novolen® 2500 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | |
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe) Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Annealed; ISO 75-2A |
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.0 °C | 172 °F | Annealed; ISO 75-2A |
Total Lacqrene® 6631 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |