Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 180 µm/m-°C @Temperature 23.0 - 100 °C |
100 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 23.0 - 100 °C |
100 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
|
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | ASTM D696 |
Manifattura Cattaneo PE UMW Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | ASTM D696 |
IPB Bicell® Cellular Polypropylene Sheet Extruded, layered PP sheet, with a cellular core layer. Attributes include:Enhanced strength/thickness ratioOmni-directional flexural stresistanceHigh compression strengthWide variety of finishesRe.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Total 50100.2 HDPE blow molding, sheet, thermoforming resin Applications: Agricultural chemical tanks, portable fuel containers, industrial parts, pallets, large foam parts, food packaging, sheet extrusion, thermoforming, truck bed liners, dunnage containers.. |
|||
CTE, linear | 180 µm/m-°C @Temperature -30.0 - 30.0 °C |
100 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 342-3.5 Room Temperature Cure Epoxy Adhesive TRA-BOND 342-3.5 room temperature curing epoxy adhesive is designed for applications which require outstanding thermal shock properties. This adhesive may be used to bond semi-porous materials such .. |
|||
CTE, linear | 180 µm/m-°C @Temperature -30.0 - 30.0 °C |
100 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 180 µm/m-°C @Temperature -30.0 - 30.0 °C |
100 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D648 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy Product Description: EPO-TEK® 301-2 is a two component optical, medical, and semiconductor grade epoxy resin, with low viscosity, long pot-life, and good handling characteristics.Advantages & Appli.. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | Silicone Property; ASTM E 831 |
Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 Fiberg.. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; JMTP P200 |
Aptek 2503R-A/B Premeasured conformal urethane coating repair kit APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components.. |
|||
CTE, linear | 180 - 230 µm/m-°C | 100 - 128 µin/in-°F | Average value: 218 µm/m-°C Grade Count:12 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
CTE, linear | 180 µm/m-°C @Temperature 20.0 °C |
100 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Total Finathene® CD 481 HDPE conduit
(discontinued **) Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
CTE, linear | 180 - 230 µm/m-°C | 100 - 128 µin/in-°F | Average value: 206 µm/m-°C Grade Count:17 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 180 µm/m-°C | 100 µin/in-°F | Silicone Property; ASTM E 831 |
Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty.. |