Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IDI Composites 48-50 Thermoset Polyester, Molding

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer IDI Composites
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IDI Composites 48-50 Thermoset Polyester, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moderate strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.93 g/cc
0.0697 lb/in³
Water Absorption 0.11 %
0.11 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
ASTM D2583
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 14.0 GPa
2030 ksi
ASTM D790
Compressive Strength 165 MPa
23900 psi
ASTM D695
Izod Impact, Notched 2.90 J/cm
5.43 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
Arc Resistance 190 sec
190 sec
ASTM D495