Excalibar ExCal® 100 Calcium Carbonate CaCO3 Powder

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Excalibar Minerals LLC
Trade Name ExCal®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Excalibar ExCal® 100 Calcium Carbonate CaCO3 Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other applications.Information provided by Excalibar Minerals LLC.
Physical Properties Metric English Comments
Specific Gravity 2.70 g/cc
2.70 g/cc
Bulk Density 1.28 g/cc
0.0463 lb/in³
Loose
1.60 g/cc
0.0579 lb/in³
Packed
Moisture Absorption 0.1 %
0.1 %
Particle Mesh Size 200 Mesh
200 Mesh
70.00% passes
pH 8.2
8.2
Component Elements Properties Metric English Comments
Al2O3 0.030 %
0.030 %
Fe2O3 0.060 %
0.060 %
SiO2 1.3 %
1.3 %
Descriptive Properties Value Comments
Acid Solubility 97
CaCO3 wt% 97
MgCO3 wt% 0.9
R2O3 wt% 0.7