Electrical Properties Metric English Comments
Dielectric Strength 12.6 kV/mm
320 kV/in
Short Time; ASTM D149
Plenco 7300 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
IDI Composites 48-50 Thermoset Polyester, Molding
Moderate strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer.
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
IDI Composites E-207 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
IDI Composites M-102 Thermoset Polyester, Molding
Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer.
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
IDI Composites W-102 Thermoset Polyester, Molding
Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer.
Dielectric Strength 12.6 kV/mm
320 kV/in
Short Time; ASTM D149
Plenco 1501 Polyester, Briquette, Compression Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
Dielectric Strength 12.6 kV/mm
320 kV/in
Short Time; ASTM D149
Plenco 1508 Polyester, Briquette, Injection Molded
PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl..
Dielectric Strength 12.6 kV/mm
320 kV/in
Short Time; ASTM D149
Plenco 2571 Phenolic, Granular, Transfer Molded
PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde..
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149
Devcon Tile Adhesive Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Dielectric Strength 12.6 - 13.8 kV/mm
320 - 350 kV/in
Step by Step
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..