Network Polymers Softflex® 7210 Black

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Network Polymers
Trade Name Softflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Softflex® 7210 Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Thickness 3.17 mm
0.016 - 0.018 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm

@Thickness 3.17 mm
0.014 - 0.016 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 3.1 g/10 min

@Load 1.00 kg,
Temperature 235 °C
3.1 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
19.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
19.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
28.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
28.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 77
67 - 77
Instantaneous; ASTM D2240
Tensile Strength, Yield 9.65 MPa
1400 psi
chs 20 in/min; ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
Tear Strength 43.8 kN/m
250 pli