Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 48.3 MPa @Temperature -55.0 °C |
7010 psi @Temperature -67.0 °F |
Lap Shear |
Henkel Hysol EA 9696 Film Adhesive Second generation, moisture-resistant, toughened 250°F / 121°C service, modified epoxy film. Qualified to BMS 5-101 and BMS 5-129. Data from .060 psf, 300 g / m2.Applications: Composite Bondin.. |