Material Notes:
Two-part, elevated cure, unfilled, low viscosity adhesive with structural properties to 400°F / 204°C.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding
Physical Properties Metric English Comments
Storage Temperature 25.0 °C
77.0 °F
Mechanical Properties Metric English Comments
Compressive Strength 96.6 MPa
14000 psi
Adhesive Bond Strength 13.8 MPa
<br>@Temperature 93.0 °C
2000 psi
<br>@Temperature 199 °F
Tensile Lap Shear
17.2 MPa
<br>@Temperature -55.0 °C
2490 psi
<br>@Temperature -67.0 °F
Tensile Lap Shear
20.7 MPa
<br>@Temperature 25.0 °C
3000 psi
<br>@Temperature 77.0 °F
Tensile Lap Shear
Peel Strength 2.80 kN/m
16.0 pli
Bell Peel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Processing Properties Metric English Comments
Cure Time 60.0 min
<br>@Temperature 93.0 °C
1.00 hour
<br>@Temperature 199 °F
Pot Life 480 min
480 min
Descriptive Properties Value Comments
Consistency Low Viscosity
Form 2 parts
Mix Ratio, Part A:Part B 100:36
Peel Strength Low