Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 20.7 MPa @Temperature -55.0 °C |
3000 psi @Temperature -67.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9321 Paste Adhesive System Thixotropic adhesive that yields tough, durable bonds over a wide temperature range.Applications: Potting Structural Repair |
|||
Adhesive Bond Strength | 20.7 MPa @Temperature 93.0 °C |
3000 psi @Temperature 199 °F |
Tensile Lap Shear |
Henkel Hysol EA 9390 Paste Adhesive System Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.Applications: Structural Bonding Low Viscosity Wet Lay-Up Composite Bonding |
|||
Adhesive Bond Strength | 20.7 MPa @Temperature 25.0 °C |
3000 psi @Temperature 77.0 °F |
Tensile Lap Shear |
Henkel Hysol EA 9396/C-2 Paste Adhesive System Two-part, elevated cure, unfilled, low viscosity adhesive with structural properties to 400°F / 204°C.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding |