Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 3490-01G meets the requirements of FDA Regulation 21 CFR 177.1520.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 160 °C
320 °F