Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gichem GILAC A070V3C Acrylonitrile Butadiene Styrene  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gichem GILAC A070V3C Acrylonitrile Butadiene Styrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ABS glass fiber filled, excellent mechanical properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
0.450 J/cm

@Temperature 0.000 °C
0.843 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
216 °F
ASTM D648
Vicat Softening Point 100 °C
212 °F
ASTM D1525/A
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Flammability Test 90
90
[°C] Bilia; IEC 331
Oxygen Index 19 %
19 %
ASTM D2863
Glow Wire Test 650 °C
1200 °F
IEC 695-2-1
Processing Properties Metric English Comments
Middle Barrel Temperature 220 °C
428 °F
Mold Temperature 50.0 - 60.0 °C
122 - 140 °F
Drying Temperature 80.0 °C
176 °F
2 hours