Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Izod Impact, Notched | 0.450 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.843 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Plenco 50015 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 0.000 °C |
0.843 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Gichem GILAC A070V3C Acrylonitrile Butadiene Styrene
(discontinued **) ABS glass fiber filled, excellent mechanical properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256A |
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
Izod Impact, Notched | 0.450 - 0.470 J/cm @Temperature -40.0 - -20.0 °C |
0.843 - 0.881 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.460 J/cm Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -40.0 °C |
0.843 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
BASF Capron® 8202 NL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
BASF Capron® B135QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Kolon KOCETAL® LF701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -20.0 °C |
0.843 ft-lb/in @Temperature -4.00 °F |
ASTM D256-03 |
Ipiranga Petrochem PCC 0742 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0952 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.450 - 0.500 J/cm | 0.843 - 0.937 ft-lb/in | ASTM D256 |
Loxim 330 12V0 Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | >= 0.450 J/cm | >= 0.843 ft-lb/in | Method A; ASTM D 256 |
Karina E 854-10/150-A-ERYB White PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RL4040HSUV PA 66 LNP* LUBRICOMP* RL4040HSUV is a compound based on Nylon 66 containing 20% PTFE. Added features of this grade include: Heat Stabilized, UV Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 0.000 °C |
0.843 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 0.000 °C |
0.843 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp ZZ006 PPE+PS LNP THERMOCOMP* ZZ006 is a compound based on PPE+PS Blend resin containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Asia Pacific) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 (Europe-Africa-Middle East) NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM340S4 Acetal, 20% Glass beads Reinforced 20% Glass beads reinforced polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB351I6 Nylon 6, 30% Glass Fiber and Mineral 30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 603 Blow Molding Polypropylene Description: H 603 is a low melt flow rate homopolymer used for general purposes. This resin is designed for blow moulding and extrusion applications. H 603 exhibits excellent processability, excell.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | |
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.450 J/cm @Diameter 3.17 mm, Temperature -20.0 °C |
0.843 ft-lb/in @Diameter 0.125 in, Temperature -4.00 °F |
bar; ASTM D256 |
BP Amoco Acctuf® 3434 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High gloss, Nucleated, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded s.. |