Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 212 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
B
Plastcom SLOVAMID 6 LI PA6, improved strength
FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme..
Vicat Softening Point 100 °C
212 °F
Rate A; ISO 306/A50
Premix Thermoplastics PRE-ELEC® PE 1313  (discontinued **)
PRE-ELEC PE 1313 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 13..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Chevron Phillips 4538B LDPE Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 05200Characteristics: Good Flexibility, Moderate Flow, Moderate Warping Resistance, Good Mold Release, Excellent ESCRApplications:Perso..
Vicat Softening Point 100 - 103 °C
212 - 217 °F
Average value: 102 °C Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Global GP-150 High Impact Polystyrene
High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys
Vicat Softening Point 100 °C
212 °F
Ineos ABS Lustran® H607AS
Contains antistatic additives,Property data per ISO test methods.
Vicat Softening Point 100 °C

@Load 1.00 kg,
Thickness 3.17 mm
212 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
IRPC Polimaxx Polene GP150 Polystyrene
APPLICATIONS: INJECTION MOULDING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY WARE, etc.
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Lucky EG-930 Acrylic, Injection Grade
Injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Lucky IG-840 Acrylic, Injection Grade
General purpose injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and col..
Vicat Softening Point 100 °C

@Load 5.00 kg
212 °F

@Load 11.0 lb
50°C/h; ASTM D1525
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Vicat Softening Point 100 °C

@Load 5.00 kg
212 °F

@Load 11.0 lb
LATI Latiohm 36/07 PD01 G/20 ABS, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor..
Vicat Softening Point 100 °C
212 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ..
Vicat Softening Point 100 °C
212 °F
Rate B/120; ISO 306
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific)
PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.
Vicat Softening Point 100 °C

@Load 5.10 kg
212 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution Novodur® E309 ABS
Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution
Vicat Softening Point 100 °C
212 °F
B/120; ISO R306
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Vicat Softening Point 100 °C
212 °F
B/120; ISO R306
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant
Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries.
Vicat Softening Point 100 °C
212 °F
ISO 306
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film
Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l...
Vicat Softening Point 100 °C
212 °F
ASTM D1525
PlastxWorld CEVIAN® SERG1 10% GF ABS
Glass fiber reinforced and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Toyobo A2080A Thermoplastic Polyurethane Elastomer, Injection Grade
Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe..
Vicat Softening Point 100 °C
212 °F
Conditioned 4 hours @ 70°C (158°F); ASTM D1525
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Chevron Phillips Marlex® 5104 LDPE Blow Molding Resin
Resin Type: HomopolymerCharacteristics: High Melt Strength, Good Parison Control, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on Gloss, Long Standing ..
Vicat Softening Point 100 °C
212 °F
Loading 1, Rate A; ASTM D1525
Chevron Phillips Marlex® 7104 LLDPE Sheet Extrusion
Resin Type: Hexene CopolymerCharacteristics: Outstanding ESCRGood melt strengthExcellent flexibilityGood processabilityGood glossHigh COFApplications: Landfill coversFlat and round-die productsCoext..
Vicat Softening Point 100 °C

@Load 1.00 kg,
Thickness 3.17 mm
212 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Diamond Polymers SAN 300 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Vicat Softening Point 100 °C
212 °F
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with excellent rigidity. It h..
Vicat Softening Point 100 °C
212 °F
BASF Procom® X25H 650 Polypropylene
Electrical and domestic appliances, housings where high gloss is required.Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 100 °C
212 °F
ASTM D1525
C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Vicat Softening Point 100 °C
212 °F
ASTM D-1525
Plaskolite West Optix® CA - 2000 HF-4-2 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
Vicat Softening Point 100 °C
212 °F
ASTM-D1525
Polyram BondyRam® 4001 Maleic Anhydride modified LLDPE coupling agent  (discontinued **)
Maleic Anhydride grafted linear low density polyethylene recommended as a coupling agent in PE composites with minerals and wood and compatibilizer in PE/PA blendsInformation provided by Polyram Ram..
Copyright © lookpolymers.com All Rights Reserved