Gharda Chemicals GATONE™ 5700 Polyetheretherketone (PEEK)  (discontinued **)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gharda Chemicals GATONE™ 5700 Polyetheretherketone (PEEK)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric Strength, Volume Resistivity, Tracking Resistance Excellent Radiation Resistance Applications:Medical appliances including implantationAerospace applicationEngineering applications like compressor plates, valve seats, moving parts for textile machines Electrical and communication cables Scientific laboratory instruments Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
24 Hours; ASTM D570
Melt Flow 45.5 - 91 g/10 min

@Load 5.00 kg,
Temperature 380 °C
45.5 - 91 g/10 min

@Load 11.0 lb,
Temperature 716 °F
6`; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
ASTM D785
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Tensile Modulus 3.80 GPa
551 ksi
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 3.60 GPa
522 ksi
ASTM D790
Izod Impact, Notched 0.440 J/cm
0.824 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Use; UL-746B
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
ASTM D648
Glass Transition Temp, Tg 148 °C
298 °F
ASTM D3482
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
UL 94
Oxygen Index 40 %
40 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Dissipation Factor 0.0030

@Frequency 60 Hz
0.0030

@Frequency 60 Hz
ASTM D150
Comparative Tracking Index 150 V
150 V
ASTM D3638