Dow Corning 193C Fluid

Category Fluid
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 193C Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning ® 193C Fluid is a silicone glycol copolymer.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
Viscosity Measure 260 cSt
260 cSt
kinetic/kinematic
Thermal Properties Metric English Comments
Flash Point 113 °C
235 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 30.0 Month
30.0 Month
Descriptive Properties Value Comments
Cloud Point (°C) 95-100