Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PP7085E1 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP7085E1 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applications like disposable houseware, consumer products, containers and rigid packaging applications.Availability: Africa & Middle East and Europe Features:AntistaticControlled RheologyHigh Flow Nucleated Uses: Containers Industrial ApplicationsPailsRigid Packaging Tool/Tote Box Processing Method: Injection Molding and CompoundingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 230 °C
75 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ISO 868
Tensile Strength, Yield 23.0 MPa
3340 psi
ISO 527-2/50
Elongation at Yield 5.0 %
5.0 %
ISO 527-2/50
Tensile Modulus 1.15 GPa
167 ksi
ISO527-2/1
Flexural Modulus 1.12 GPa
163 ksi
ISO 178
Izod Impact, Notched (ISO) 5.46 kJ/m²
2.60 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.399 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.504 J/cm²

@Temperature 0.000 °C
2.40 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
0.756 J/cm²

@Temperature 22.8 °C
3.60 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 322 °C
612 °F
ISO 3146
Crystallization Temperature 253 °C
487 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-2/A
Vicat Softening Point 147 °C
297 °F
ISO 306/A50
Copyright © lookpolymers.com All Rights Reserved