Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 253 °C | 487 °F | ISO 3146 |
ExxonMobil PP1055E2 Polypropylene Homopolymer Product Description: A nucleated homopolymer resin with good flowability and antistatic properties. It is designed for molding of media packaging, containers and other articles requiring fast moldi.. |
|||
Crystallization Temperature | 253 °C | 487 °F | ISO 3146 |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |
|||
Crystallization Temperature | 253 °C | 487 °F | ISO 3146 |
ExxonMobil PP7085E1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica.. |