Polymer Property : Charpy Impact, Notched = 3.60 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.756 J/cm²

@Temperature 22.8 °C
3.60 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
ExxonMobil AP03B Polypropylene Impact Copolymer
Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio..
Charpy Impact, Notched 0.756 J/cm²

@Temperature 0.000 °C
3.60 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
ExxonMobil PP7043L1 Polypropylene Impact Copolymer
Product Description: An impact copolymer resin characterized by medium flow. It is suitable for molding applications like consumer products, containers and rigid packaging applications.Availability..
Charpy Impact, Notched 0.756 J/cm²

@Temperature 22.8 °C
3.60 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
ExxonMobil PP7085E1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica..