Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 322 °C | 612 °F | |
Shamrock Technologies NanoFLON® P 39B Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Melting Point | 322 °C | 612 °F | |
Shamrock Technologies NanoFLON® P 63B Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-201 PTFE Fine Powder Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-202 PTFE Fine Powder Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-203 PTFE Fine Powder Usage: The resin is used to process capillary tube, thin-wall tube, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside... |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-204 PTFE Fine Powder Usage: The resin is mainly used for elastic tape, capillary tube, and the unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE s.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-21 PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-21A PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-21B PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-21C PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in .. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles) Usage: The resin can be used as the general required electric source, which is suitable for making film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop, fillin.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as the packing products resource and packing pelletized resource, which can be processed to film, the products of thin wall, seal, gasket, club, panel, tube, axletree.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-205 PTFE Fine Powder Usage: The resin is used to process two-side draw film, capillary tube, thin-wall tube, sheet, small-diameter rod, elastic belt and unsintered tape etc.Packing: PTFE is packed in double layer PVC ba.. |
|||
Melting Point | 322 °C | 612 °F | ISO 3146 |
ExxonMobil PP7011L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent low-temperature impact strength. It is suitable for cables, pipes, profiles, sheets .. |
|||
Melting Point | 322 °C | 612 °F | ISO 3146 |
ExxonMobil PP7033L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like.. |
|||
Melting Point | 322 °C | 612 °F | ISO 3146 |
ExxonMobil PP7043L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin characterized by medium flow. It is suitable for molding applications like consumer products, containers and rigid packaging applications.Availability.. |
|||
Melting Point | 322 °C | 612 °F | ISO 3146 |
ExxonMobil PP7085E1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica.. |
|||
Melting Point | 322 - 332 °C | 612 - 630 °F | |
Shandong Dongyue Polymer DF-101 PTFE Molding Powder (Medium Particle Size) Usage: Can be processed to film, sheet, rob, gasket, axletree and presintered material.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE shou.. |