Polymer Property : Melt Flow = 75 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 230 °C
75 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Phillips 66 COPYLENE® CR750CL-02 Polypropylene, Random Copolymer, NX-8000 based
COPYLENE™ CR750CL-02 is an easy molding, high melt flow random copolymer that has good see-through and contact clarity in injection molding applications and is formulated with advanced technology. ..
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 230 °C
75 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Phillips 66 COPYLENE® CR750CLS Polypropylene Random Copolymer
Description: COPYLENE® CR750CLS is a clarified random copolymer specially designed and formulated for clear injection molding applications and is formulated with antistat and lube for excellent mol..
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 380 °C
75 g/10 min

@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)  (Unverified Data**)
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn..
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin  (discontinued **)
Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e..
Melt Flow 75 g/10 min

@Load 5.00 kg,
Temperature 316 °C
75 g/10 min

@Load 11.0 lb,
Temperature 600 °F
ASTM D1283
Chevron Phillips Ryton® P-4 Polyphenylene Sulfide Resin  (discontinued **)
Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R..
Melt Flow 75 g/10 min

@Load 5.00 kg,
Temperature 316 °C
75 g/10 min

@Load 11.0 lb,
Temperature 601 °F
Procedure B; ASTM D1283
Chevron Phillips Ryton® P-4-60 Polyphenylene Sulfide Resin  (discontinued **)
Tan Color Polyphenylene Sulfide ResinRyton® P-4-60 is supplied as pellets. The powder form is P-4. Ryton® PPS exhibits excellent thermal stability and chemical resistance and is suitable for a v..
Melt Flow 75 g/10 min

@Load 5.00 kg,
Temperature 270 °C
75 g/10 min

@Load 11.0 lb,
Temperature 518 °F
Calculated from MVR using melt density; ISO 1133
Lanxess Durethan® A 30 S 000000 Nylon 66
PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 230 °C
75 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Multibase Multi-Flex® TEA 4001-35 Natural TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 380 °C
75 g/10 min

@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s..
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 380 °C
75 g/10 min

@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci..
Melt Flow 75 g/10 min

@Load 10.0 kg,
Temperature 250 °C
75 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 75 g/10 min

@Load 5.00 kg,
Temperature 250 °C
75 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A..
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex MONPRENE® MP 2820M Thermoplastic Elastomer
Information provided by Teknor Apex Company
Melt Flow 75 g/10 min

@Load 10.0 kg,
Temperature 250 °C
75 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 75 g/10 min

@Temperature 230 °C
75 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Formosa Plastics Formolene® 2575N injection Molded Polypropylene
Impact Copolymer for High Speed injection Molded ApplicationsFormolene® 2575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging, ..
Melt Flow 75 g/10 min

@Temperature 230 °C
75 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene
Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,..
Melt Flow 75 g/10 min
75 g/10 min
ASTM D1238
Total PPC 5946WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 5946WZ is a nucleated impact copolymer with a Melt Flow index of 75 g/10 min.TOTAL Polypropylene 5946WZ is characterized by very low warpage, improved stiffness, a..
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 230 °C
75 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
ExxonMobil PP7085E1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica..
Melt Flow 75 g/10 min

@Load 10.0 kg,
Temperature 220 °C
75 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Melt Volume Rate (ml/10 min); ISO 1133
Chi Mei Polylac® PA-756H ABS - High Flow
Super high flow
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
"E"; ASTM D1238
Aaron Industries AAROPRENE® ATPR 1000 70A Elastomeric Compound
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Melt Flow 75 g/10 min

@Temperature 230 °C
75 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Formosa Plastics Formolene® 6375N Impact Copolymer Polypropylene
Impact Copolymer For High Speed Injection Molded Applications Formolene® 6375N is a very high melt flow, low impact copolymer of polypropylene. It is designed for such applications as packaging, ho..
Melt Flow 75 g/10 min

@Load 2.16 kg,
Temperature 380 °C
75 g/10 min

@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)  (Unverified Data**)
Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. ..