Henkel Hysol PL 7000 Film Adhesive

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol PL 7000 Film Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Epoxy film adhesive formulated to provide excellent performance properties in composite bonding, and has excellent results on composite surfaces that have been exposed to bond shop environments and may have absorbed moisture. Excellent fracture toughness (G1C) over composite surfaces exhibiting cohesive failure patterns, indicating superior adhesion characteristics. Qualified at Boeing.Application: Composite Surfacing
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 7.40 MPa
1070 psi
Flatwise
Adhesive Bond Strength 9.00 MPa

@Temperature 132 °C
1310 psi

@Temperature 270 °F
Lap Shear
26.2 MPa

@Temperature -55.0 °C
3800 psi

@Temperature -67.0 °F
Lap Shear
31.0 MPa

@Temperature 25.0 °C
4500 psi

@Temperature 77.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Glass Transition Temp, Tg 62.5 °C
145 °F
dry
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature 177 °C
1.00 - 2.00 hour

@Temperature 351 °F
90.0 - 120 min

@Temperature 121 °C
1.50 - 2.00 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Out-Time (days) 30
at 25°C