Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.756 J/cm² @Temperature 22.8 °C |
3.60 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
ExxonMobil AP03B Polypropylene Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio.. |
|||
Charpy Impact, Notched | 0.756 J/cm² @Temperature 0.000 °C |
3.60 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
ExxonMobil PP7043L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin characterized by medium flow. It is suitable for molding applications like consumer products, containers and rigid packaging applications.Availability.. |
|||
Charpy Impact, Notched | 0.756 J/cm² @Temperature 22.8 °C |
3.60 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
ExxonMobil PP7085E1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica.. |