Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 147 °C @Load 5.001 kg |
297 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANTEC PC S75R GF20 Polycarbonate, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East) LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat. |
|||
Vicat Softening Point | 147 °C | 297 °F | |
Dow Isoplast® 2532 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 2532 resin is a clear amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include clarity, excelle.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East) LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance. |
|||
Vicat Softening Point | 147 °C | 297 °F | |
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade
(discontinued **) Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui.. |
|||
Vicat Softening Point | >= 147 °C | >= 297 °F | |
Kazanorgsintez PC-007 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Vicat Softening Point | >= 147 °C | >= 297 °F | |
Kazanorgsintez PC-010 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of die-casting.Information Provided by Kazanorgsintez |
|||
Vicat Softening Point | >= 147 °C | >= 297 °F | |
Kazanorgsintez PC-022 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of die-casting.Information Provided by Kazanorgsintez |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Vicat Softening Point | 147 °C | 297 °F | ASTM D1525-97 |
Ipiranga Petrochem PCC 0412 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1201-22 Polycarbonate Resin Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Vicat Softening Point | 147 °C | 297 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 147 °C | 297 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525; ISO 360/B50 |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Vicat Softening Point | 147 °C | 297 °F | ISO 306/B50 |
Styron CALIBREâ„¢ 301-58 LT Polycarbonate Resin Overview: CALIBREâ„¢ 301-58 LT is a high light transmission, high-flow polycarbonate resin for injection molding applications.Main Characteristics:High light transmissionHigh flow for injection m.. |
|||
Vicat Softening Point | 147 °C | 297 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 147 °C | 297 °F | ASTM D1525 |
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Vicat Softening Point | 147 °C | 297 °F | |
Covestro Makrolon® 2808 Polycarbonate, Injection Grade Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Vicat Softening Point | 147 °C @Load 1.02 kg |
297 °F @Load 2.25 lb |
ASTM D1525 |
Carmel Olefins CAPILENE® HT 75 A Polypropylene Impact Copolymer Description: CAPILENE® HT 75 A is a nucleated and antistatic high flow impact copolymer for injection molding. It is characterized by improved stiffness, medium impact resistance and good organol.. |
|||
Vicat Softening Point | 147 °C @Load 1.02 kg |
297 °F @Load 2.25 lb |
ISO 306 |
Arkema Group OREVAC® CA 100 Grafted Maleic Anhydride Polypropylene OREVAC® CA 100 is a chemically functionalized polypropylene with a high content of maleic anhydride. Grafting on polypropylene backbone is achieved with a processing technology which allows to opti.. |
|||
Vicat Softening Point | 147 °C | 297 °F | 10 N; ASTM D1525 |
Braskem CP 741 Blow Molding Polypropylene Description: CP 741 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and general purpose additive package. CP 741 presents low odor/taste transfer, high mel.. |
|||
Vicat Softening Point | 147 °C | 297 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |