Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excellent drawability, makes this a very versatile packaging film resin. LL3001.63 is formulated for blown film extrusion.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoProcessing Aid: Yes Thermal Stabilizer: YesApplications: Freezer FilmHeavy Duty BagsIce BagsStretch FilmTrash BagsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ExxonMobil method
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa
1500 psi
ASTM D882
Film Elongation at Break, MD 500 %
500 %
ASTM D882
Film Elongation at Break, TD 840 %
840 %
ASTM D882
Puncture Energy 3.05 J
2.25 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 440 g
440 g
ASTM D1922
Elmendorf Tear Strength TD 740 g
740 g
ASTM D1922
Dart Drop Test 140 g
0.309 lb
ASTM D1709A
Film Tensile Strength at Break, MD 57.9 MPa
8400 psi
ASTM D882
Film Tensile Strength at Break, TD 48.3 MPa
7000 psi
ASTM D882
1% Secant Modulus, MD 200 MPa
29000 psi
ASTM D882
1% Secant Modulus, TD 234 MPa
34000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 255 °C
<= 491 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Gloss 49 %
49 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 9 lbf
ExxonMobil Method