Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 200 MPa | 29000 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LD 136.MV Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LD 136.NI Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
LyondellBasell Petrothene® NA960070 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
LyondellBasell Petrothene® NA960083 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74838 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and medium antiblock. Films produced with this re.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74845 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74845 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and high antiblock. Films produced with this resi.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPE Appl.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film This LLDPE is tailored for cast film applications that require:Good stiffness at thin gaugesGood drawdownExcellent processabilityCan be used singly or in blends with LDPE or HDPEAvailable with slip .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | Cast Film at 1.25 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7120X Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade) Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem Green PE SLL218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL218 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for cast film extrusion. Films obtained with this product show a good processing performance balanced with .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem Green PE SLL218/21 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Lower greenhouse gas emissions100% made from renewable raw materialsPerformance and Competitiveness: Green Polyethylene has the same characteristics as petrochemical polyethyleneApplications: Line.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol® process technology. It shows low haze and high clarity associated with good balance of mechanical properties, processing .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM-D882 |
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this p.. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem LL118 Blown Film Extrusion Linear Low Density Polyethylene Description: LL218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and .. |
|||
1% Secant Modulus, MD | 200 MPa | 29000 psi | ASTM D882 |
Braskem LL218 Cast Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |