Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
Westlake LF2040 Hexene Linear Low Density Polyethylene
Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
Westlake LF2050 Hexene Linear Low Density Polyethylene
Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 20-05CH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin
Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade)
Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018MK Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin
Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawn down to thing gauges.Availability: Latin America, North America and S..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LL 1001x26 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LL 1001x72 Blown Film Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LL 1001x74 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LL 1001x76 Blown Film Resin
LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin
Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin
Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Dow FLEXOMER™ ETS-9064 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
Dow FLEXOMER™ ETS-9064 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper..
Film Tensile Strength at Yield, MD 9.65 MPa
1400 psi
ASTM D882
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin
Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p..