Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LC-0517-A LDPE Extrusion Resin Excellent adhesion, High drawdown, Excellent sealabilityApplications: Dry soup pouches, Powdered drink pouches, Pharmaceutical packaging, Potato chip bags, Flexible and snack food packagingAdditives.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealabilityApplications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper co.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D792 |
NOVA Chemicals Surpass® FPs317-A Octene sLLDPE Film Resin Features: Exceptional puncture resistanceVery good tear propertiesLow gel levelExcellent optical properties Excellent elongation characteristics Easy to process, no drying required Applications: Cas.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Vytek™ V208C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | Base Resin; ASTM D4833-89 |
Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additiveCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ExxonMobil Method |
ExxonMobil LL 3002.32 Cast Film Resin
(discontinued **) LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, .. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505-60T |
Chevron Phillips 1025 Extrusion Coating Resin
(discontinued **) Resin Type: Speed Resin, Base Resin Type - Chevron PE1017Characteristics: Excellent Processability at 570-620°F (300-325°C) Melt, Good Adhesion at Low Coating Weights and High Speed Lines, Low COF.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505-60T |
Chevron Phillips MarFlex® 1010 LDPE Extrusion Coating Resin
(discontinued **) Resin Type: High Speed ResinCharacteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down ResinApplications: Food Packaging, LaminationsData provided by Chevron Che.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Eastman 808A Polyethylene
(discontinued **) Low density polyethylene 808A is a general-purpose formulation used for injection molding and general-purpose extrusion.Unless otherwise noted, all tests are run at 23°C and 50% RH.Information from.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | Exxon Method |
ExxonMobil Exceed™ 363C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 363C32 resin have outstanding tensile properties and.. |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 107-276 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 107-278 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 108-276 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 - 0.925 g/cc | 0.0331 - 0.0334 lb/in³ | |
Kazanorgsintez 162-280 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505-98 |
Ipiranga Petrochem LBH 0117 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505-98 |
Ipiranga Petrochem LBH 0120 BP LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | |
LyondellBasell Lupolen® 1800 S LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake Hifor Xtreme SC74845 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74845 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and high antiblock. Films produced with this resi.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 1003 LDPE Injection Molding Resin Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: HousewaresTamper evident, snap-on capsWine bottle sleeve capsInfo.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ExxonMobil NTX™ NTX 101 Super Strength Film Resin NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2267G Linear Low Density Polyethylene A high performance stretch film resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM-D792 |
Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer LBH0120BPS is a LLDPE Hexene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as s.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ExxonMobil Method |
ExxonMobil LD 206.48 Extrusion Coating Resin
(discontinued **) LD 206.48 is a extrusion coating grade, having good organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers.Information provided by ExxonMobil Chemic.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Huntsman PE2038 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High mechanical flexing properties, excellent processability, good stress crack resistance, and very good low temperature strength.Applications: Injection mol.. |
|||
Density | 0.917 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Huntsman PE2049 Injection Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good molding processability, produces parts that are flexible, and show excellent flatness in large projected areas.Applicat.. |