Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 740 g | 740 g | ASTM D1922 |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Elmendorf Tear Strength TD | 740 g | 740 g | ASTM D1922 |
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell.. |
|||
Elmendorf Tear Strength TD | 740 g | 740 g | ASTM D1922 |
Huntsman Rexell® L3102 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Good impact and puncture resistance with excellent optics and sealability.Applications: Laminated and coextruded films for .. |