Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 234 MPa | 34000 psi | ASTM D882 |
LyondellBasell Petrothene® NA960000 Low Density Polyethylene ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif.. |
|||
1% Secant Modulus, TD | 234 MPa | 34000 psi | ASTM D882 |
LyondellBasell Petrothene® NA960070 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
1% Secant Modulus, TD | 234 MPa | 34000 psi | ASTM D882 |
LyondellBasell Petrothene® NA960083 Low Density Polyethylene ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un.. |
|||
1% Secant Modulus, TD | 234 MPa | 34000 psi | ASTM D882 |
ExxonMobil LLDPE LL 3001.63 Linear Low Density Polyethylene Resin Product Description: LL 3001.36 is a hexane copolymer LLDPE film resin. Films made from this resin have outstanding tensile and toughness properties. Superior strength properties, along with excell.. |